MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Borealis Polycure™ PC780 Flame Retardant Crosslinking Polyethylene Compound for Low Voltage Insulation  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Polycure PC780 is a natural, chemically crosslinking polyethylene compound designed for flame retardant low voltage wire insulation and jacketing. PC780 contains a halogen-based, flame retardant additive package designed to reduce normal PE flame spread characteristics and achieve a VW-1 flame resistant rating on 14 AWG wires and larger.

Polycure PC780 is recommended for use in 600 volt power cable and control cable applications. It is also UL approved in applications with oil and gasoline exposure and is suitable for 90°C service in wet conditions.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 1926 psiHeat Aging (7 days at 121°C); ASTM D412
 2140 psiASTM D412
Elongation at Break 315 %Heat Aging(7 days at 121°C); ASTM D412
 350 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.10e+16 ohm-cmASTM D257
Dielectric Constant 2.6
@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 840 V/milAt 40 mils; ASTM D149
Dissipation Factor 0.00050
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 27 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature >= 116 °C
Melt Temperature >= 121 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Casico™ FR4807 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Borealis PC0787 Polyethylene Insulation Compound, Crosslinkable
Borealis Casico™ FR4804 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Borealis Casico™ FR4803 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Borealis RF365MO Polypropylene

PBOREA185 / 27492

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.