MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 30 pcf
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Baydur 645 is a rigid polyurethane structural foam system used in the reaction injection molding (RIM) process.

Properties / Applications: Baydur 645 is a rigid polyurethane structural foam system used in the reaction injection molding (RIM) process. The system is supplied as two reactive liquid components. Component A is a polymeric diphenylmethane diisocyanate (PMDI), and Component B is a formulated polyol system containing no CFC- or HCFC-blowing additives. The Baydur 645 system is used to produce foam cores for composite applications, such as water skis, agricultural and construction equipment, and various components for the transportation and marine markets. As with any product, use of the Baydur 645 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.480 g/cc
@Thickness 6.35 mm
ASTM D792
 0.480 g/cc
@Thickness 12.7 mm
ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55
@Thickness 6.35 mm
ASTM D2240
 55
@Thickness 12.7 mm
ASTM D2240
Tensile Strength at Break 10.0 MPa
@Thickness 12.7 mm
ASTM D638
 12.0 MPa
@Thickness 6.35 mm
ASTM D638
Elongation at Break 7.0 %
@Thickness 6.35 mm
ASTM D638
 9.0 %
@Thickness 12.7 mm
ASTM D638
Flexural Strength 16.5 MPa
@Thickness 6.35 mm
ASTM D790
 20.0 MPa
@Thickness 12.7 mm
ASTM D790
Flexural Modulus 517 MPa
@Thickness 12.7 mm
ASTM D790
 572 MPa
@Thickness 6.35 mm
ASTM D790
Compressive Strength 10.3 MPa
@Thickness 6.35 mm
ASTM D695
 10.3 MPa
@Thickness 12.7 mm
ASTM D695
Charpy Impact Unnotched 8.82 kJ/m²
@Thickness 6.35 mm
 9.03 kJ/m²
@Thickness 12.7 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 20 pcf
BCC Products MB 1200 Polyurethane Foam Modeling Board
Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 15 pcf
Covestro Baynat® 3002 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3818 FST Polyurethane Foam

PCOVEST0085 / 201868

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.