MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 2307 Masking Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Masking Tape 2307 is a general purpose masking tape for holding, bundling, sealing, general paint masking and a vast number of other jobs where a pressure-sensitive tape is needed.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 5.20 milASTM D3652
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 31.0 MPaASTM D3756
Elongation at Break 8.0 %ASTM D3756
Peel Strength 1.75 plito Steel
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °Cfor 30 mins
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Adhesive TypeRubber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Copolymer Polypropylene
RTP Company PermaStat® 1000 U LF  Polybutylene Terephthalate (PBT) Anti-Static - Low Flow
Reltek BONDiT™ B-481 Adhesive, Sealant & Coating System
Epsan Eplon 6 NC Q101 Polyamide 6
Epsan Eplon 6 IMP NC Q1A501 Polyamide 6

PMM33980 / 168727

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.