MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Aptek DIS-A-PASTE 2001-PMF Thermally conductive urethane adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Premixed-frozen, thermally conductive urethane adhesive
DIS-A-PASTE 2001-PMF is a one component, premixed-frozen, mineral filled, and off-white electrically insulating soft urethane paste adhesive. It is designed to bond many dissimilar substrates and dissipate device generated heat. DIS-A-PASTE 2001-PMF is a 100% solid, solvent free system that will not form voids during cure or outgas after being fully cured. This product is a non-TDI based urethane system which has reversion resistance and physical stability when subjected to high heat and humidity environments. As a urethane, this system displays higher ionic purity than epoxy systems minimizing the chance of corrosion around sensitive components and circuitry.

Premixed-frozen and packaged in syringes for convenient dispensing to circuit board. Low modulus to minimize stress to sensitive components and ceramic substrates. Low Tg for excellent low temperature cycling and performance. Excellent substrate adhesion; superior to silicones. Bonds DAT-A-THERM 1000 thermally conductive urethane film to devices and substrates without loss of thermal conductivity. Product also available in 8-10 mil. bondline spacers-designated DIS-A-PASTE 2001/.01.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.10 g/ccASTM D1475
Viscosity 140000 cPASTM D1824
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83Cured property; ASTM D2240
Adhesive Bond Strength 425 psiAl-to-Al Lap Shear; Cured property; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+14 ohm-cmCured property; ASTM D257
Dielectric Constant 5.8
@Frequency 1000 Hz
Cured property; ASTM D150
Dielectric Strength 620 V/mil
@Thickness 1.27 mm
Cured; ASTM D149
Dissipation Factor 0.030
@Frequency 1000 Hz
Cured property; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 1
 147 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 2
Thermal Conductivity 9.60 BTU-in/hr-ft²-°FCured property; COLORA
Glass Transition Temp, Tg -60.0 °CCured property; JMTP P-200
Flash Point >= 200 °CASTM D92
 
Processing PropertiesOriginal ValueComments
Processing Temperature 85.0 °CCure 6 hrs
 100 °CCure 4 hrs
 125 °CCure 2 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aptek DIS-A-PASTE 2003-A/B Thermally conductive urethane adhesive
Aptek DIS-A-PASTE 2000-A/B Thermally conductive urethane adhesive
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets
Overview of materials for Thermoset Polyurethane, Adhesive

PAPTEK01 / 24163

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.