MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion SupremEX® 640XA MMC Aluminum - Silicon Carbide Metal Matrix Composite, T7, Billet
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: SupremEX® 640XA MMC is a high quality, aerospace-grade aluminum alloy (6061B) reinforced with 40 vol.% silicon carbide particles. This composite material is manufactured via powder metallurgy using a mechanical alloying process to ensure a homogeneous reinforcement distribution, providing a refined grain structure and enhanced mechanical properties. SupremEX 640XA MMC is heat treatable, offering high strength and modulus with a CTE match to nickel plating (13 ppm/°C). This material is excellent for lightweight, high-stability structural applications. Designation: 6061B/SiC/40p (3 µm).

Benefits

  • Weight saving
  • Static strength comparable to high-strength Al alloys
  • Exceptional specific stiffness for increased component stiffness
  • High fatigue resistance
  • Refined, homogeneous and stable microstructure
  • Excellent hardness, wear resistance and low friction characteristics
  • Good machinability using high-speed machining techniques
  • Superior thermal stability, with CTE match to Ni plating

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 66.7 ksi
Tensile Strength, Yield 56.6 ksi
@Strain 0.200 %
Elongation at Break 1.20 %
Modulus of Elasticity 140 GPa
Poissons Ratio 0.300
Shear Modulus 54.0 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.20 µin/in-°F
Specific Heat Capacity 0.820 J/g-°C
Thermal Conductivity 150 W/m-K
Solidus 570 °C
 
Descriptive Properties
Specific Stiffness48 GPa/g/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NBB9113j / 323542

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.