MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Selenis BONDZ BO 244 Copolyester for Coextruded Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Selenis Bondz BO 244 is a copolyester specifically designed for sealing layers in BOPET films and inhibits crystallization. Selenis has developed this bonding solution to consistently deliver excellent melt strength and exceptional heat-sealing performance. This product is formulated to provide and sustain the adhesion level crucial to the packaging integrity through the different processes of manufacturing, securing full protection of the final product. Selenis Bondz BO 244 greatly improves converting steps, such as laminating, metalizing and printing. Selenis Bondz BO 244 is an amorphous copolyester resin dedicated to twin-screw extrusion, where no drying is required prior to extrusion.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption at Equilibrium <= 0.30 %
Viscosity Test 66 - 70 cm³/gIntrinsic; ISO 1628-5
ASTM Color <= 1.0b*; ASTM D6290
 >= 63L*; ASTM D6290
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 71.0 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Drying Temperature <= 65.0 °Cto avoid chips sticking together in dryer hopper
 60.0 - 65.0 °C
@Time >=28800 sec
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C
 
Descriptive Properties
Food Approval PharmacopeiaYes
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE919 / 243417

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.