MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi FGF Recycled PC-ABS 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; ABS Polymer

Material Notes: PC-ABS is an incredibly strong material with an even higher impact resistance than regular ABS. This is a consequence of the addition of the proper amount of polycarbonate in this modification, which also creates an early perfect interlayer adhesion and a beautiful surface gloss. The above features makes PC-ABS the perfect material for mechanical parts and tools, which should be light and strong and show minimal wear after prolonged use.

Features:

  • Improved interlayer adhesion
  • High impact resistance
Colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccISO 1183
Linear Mold Shrinkage 0.0035 cm/cmISO 294
Melt Flow 0.47 g/10 min
@Load 5.00 kg,
Temperature 240 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPaISO 527
Tensile Strength, Yield 37.0 MPaISO 527
Elongation at Break 18 %ISO 527
Elongation at Yield 3.0 %ISO 527
Tensile Modulus 1900 MPaISO 527
Charpy Impact, Notched 27.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 61.7 °CISO 306
 
Processing PropertiesOriginal ValueComments
Zone 1 210 - 250 °C
Zone 2 220 - 260 °C
Zone 3 220 - 260 °C
Die Temperature 235 - 275 °C
Drying Temperature 90.0 °C<400 ppm
Dry Time 3.00 hour
 
Descriptive Properties
Mass Temperature245°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9819 / 301044

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.