MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DowAksa CarbonBond™ 100-HT Primer System
Material Notes: DowAksa CarbonBondT™ 100-HT Primer System is a rapid setting, moisture-tolerant epoxy resin system intended for priming the substrates to which a carbon fiber reinforced overwrap is about be applied. The low viscosity wets the surface rapidly and penetrates minor cracks and surface imperfections while the thixotropic nature helps to prevent running or crawling. The pot life and cure speed are tailored to permit installation of the overwrap system in as little as 1 to 2 hours after application.

Information provided by DowAksa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccPart B
 1.107 g/ccMixed
 1.143 g/ccPart A
Brookfield Viscosity 350 cPPart B; LVT#2 - 30 rpm; ASTM D2196
 650 cPMixed LVT#2 - 30 rpm; ASTM D2196
 700 cPPart A; LVT#2 - 30 rpm; ASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength <= 10.15 ksiASTM D638
Elongation at Break 2.3 %ASTM D638
Tensile Modulus 537 ksiASTM D638
Flexural Strength <= 13.35 ksi
@Strain 2.8 %
ASTM D790
Flexural Modulus 508 ksiASTM D790
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 210 °FCured; ASTM E1640
 
Processing PropertiesOriginal ValueComments
Gel Time 40.0 - 55.0 min100g
Shelf Life 24.0 MonthPart A
 24.0 MonthPart B
 
Descriptive Properties
ColorClear RedPart B
 TranslucentPart A
 Translucent RedMixed
Mix Ratio2.75:1 A:BVolume
 3.1:1 A:BWeight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWAK983 / 287930

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.