MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Selenis VENUZ BD 286 Copolyester for Cosmetics Packaging
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Selenis Venuz BD 286 has been specifically developed for the cosmetics market where exceptional clarity is combined with high performance and easy processing, allowing efficient package designs that transmit luxury. Cosmetic parts molded from Selenis Venuz BD 286 provide good chemical resistance to most ingredients used in the industry as well as good barrier properties, helping brand owners grant product safety and preservation during storage. Packaging cost may be reduced as shelf life can be maintained even without the use of additional liners. The superior clarity of the Selenis Venuz BD 286 grade allows packaging engineers to design parts with thick walls without sacrificing transparency. The combination of density and thick walls increases the weight of the package, reinforcing the consumer perception of a high-end product. Selenis Venuz BD 286 provides good impact resistance, resembling the appearance of glass with the advantage of being virtually unbreakable, allowing unique and personalized designs. The Selenis Venuz BD 286 copolyester is the ideal choice for injection molding. This material allows fast cycle times and may improve efficiency.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.730 g/cc
Density 1.28 g/ccASTM D792
Water Absorption <= 0.12 %ASTM D570
Viscosity Test 70 - 74 cm³/gIntrinsic; ISO 1628-5
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D 955
ASTM Color <= 1.0b*; ASTM D6290
 >= 68L*; ASTM D6290
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 47.3 MPa(σm); ISO 527 -1/- 2
Tensile Strength, Yield 47.0 MPa(σy); ISO 527 -1/- 2
Elongation at Break 76.7 %Nominal, (εtb); ISO 527 -1/- 2
Elongation at Yield 4.2 %(εm); ISO 527 -1/- 2
 4.2 %(εy); ISO 527 -1/- 2
Tensile Modulus 2031 MPaISO 527 -1/- 2
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 5.00 kJ/m²
@Temperature 0.000 °C
ISO 180/A
 5.60 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/A
Izod Impact, Unnotched (ISO) NB
@Temperature -30.0 °C
ISO 180/U
 NB
@Temperature 0.000 °C
ISO 180/U
 NB
@Temperature 23.0 °C
50% RH; ISO 180/U
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 58.8 °CISO 75-1/-2
Glass Transition Temp, Tg 85.0 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %
@Thickness 2.00 mm
ASTM D1003
Gloss 166 %60º; ASTM D2457
Yellow Index <= 1.0 %
@Thickness 2.00 mm
ASTM (E313-73)
Transmission, Visible 82 %
@Thickness 6.00 mm,
Wavelength 400 nm
Disk
 83 %
@Thickness 5.00 mm,
Wavelength 400 nm
Disk
 84 %
@Thickness 4.00 mm,
Wavelength 400 nm
Disk
 87 %
@Thickness 3.00 mm,
Wavelength 400 nm
Disk
 89 %
@Thickness 2.00 mm,
Wavelength 400 nm
Disk
 89 %
@Thickness 4.00 - 6.00 mm,
Wavelength 440 - 660 nm
Disk
 90 %
@Thickness 1.00 - 3.00 mm,
Wavelength 440 - 660 nm
Disk
 90 %
@Thickness 1.00 mm,
Wavelength 400 nm
Disk
 91 %
@Thickness 1.00 - 6.00 mm,
Wavelength 660 - 740 nm
Disk
UV Transmittance 70 %
@Thickness 6.00 mm,
Wavelength 370 nm
Disk
 71 %
@Thickness 5.00 mm,
Wavelength 370 nm
Disk
 76 %
@Thickness 4.00 mm,
Wavelength 370 nm
Disk
 79 %
@Thickness 3.00 mm,
Wavelength 370 nm
Disk
 80 %
@Thickness 2.00 mm,
Wavelength 370 nm
Disk
 85 %
@Thickness 1.00 mm,
Wavelength 370 nm
Disk
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °C
Drying Temperature <= 70.0 °Cto avoid chips sticking together in dryer hopper
 65.0 °C
@Time 21600 - 28800 sec
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C
 
Descriptive Properties
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE928 / 243426

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.