MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Aerafin™ 17M Propylene-based olefin polymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Eastman Aerafin™ 17M (molten) polymer is a fully saturated, low molecular weight, propylenebased olefin polymer that is compatible with a range of hydrocarbon tackifying resins and enables spraying the finished adhesive at a broad range of temperatures and operating conditions. Aerafin™ 17M polymer is characterized by consistent quality, low color, excellent thermal stability, and low odor. This product ships in molten form unless otherwise specified.

Application/Uses:

  • Hot Melt Adhesives
  • Hygiene Construction
  • Nonwovens
  • Packaging
Key Attributes:
  • Compatibility with an array of hydrocarbon tackifying resins
  • Excellent thermal stability
  • Good adhesion with excellent peel strength
  • In formulation, enables a robust adhesive system with a broad processing window and sprayability at temperatures as low as 130°C
  • Low color and odor
  • Reliable global supply
  • Requires lower tackifier loading than with most SBC-based formulations

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 1700 cP
@Temperature 190 °C
ASTM D3236
 
Mechanical PropertiesOriginal ValueComments
Penetration 20[dmm], Hardness; ASTM D5
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -38.0 °CASTM D3418
Ring & Ball Softening Point 130 °CASTM E 28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 1.0Molten
 
Descriptive Properties
AppearanceMolten/solid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
3D Systems DuraForm® PA Nylon for SLS® Systems
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting

PEATM5122 / 222316

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.