MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Semitron® CMP XL20 (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Water Absorption 0.40 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 1.7 %ASTM D 570(2)
Outgassing - Total Mass Loss 1.85 %ASTM E595
Collected Volatile Condensable Material 0.00 %ASTM E-595
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) 3.9 ppmICP/MS
Ionic Impurities - K (Potassium) 0.50 ppmICP/MS
Ionic Impurities - Fe (Iron) 1.5 ppmICP/MS
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 80ASTM D785
Hardness, Rockwell M 120ASTM D785
Tensile Strength 20000 psiASTM D638
Tensile Strength at 150°C (300°F) 15000 psiASTM D638
Tensile Strength at 65°C (150°F) 18000 psiASTM D638
Elongation at Break 10 %ASTM D638
Tensile Modulus 575 ksiASTM D638
Flexural Strength 24000 psiASTM D790
Flexural Modulus 600 ksiASTM D790
Compressive Strength 24000 psi10% Def.; ASTM D695
Compressive Modulus 400000 psiASTM D695
Shear Strength 16000 psiASTM D732
Izod Impact, Notched 2.0 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.35dry vs. steel; QTM55007
K (wear) Factor >= 1000 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 4000 psi-ft/min4:1 safety factor applied; QTM 55010
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+16 ohmASTM D257
Dielectric Constant 4.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 580 kV/inShort Term; ASTM D149
Dissipation Factor 0.026
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µin/in-°F
@Temperature -40.0 - 150 °C
ASTM E831
Thermal Conductivity 1.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 °FContinuous
Deflection Temperature at 1.8 MPa (264 psi) 532 °FASTM D648
Glass Transition Temp, Tg 527 °FAmorphous; ASTM D3418
Flammability, UL94 V-0
@Thickness 3.17 mm
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Acceptable
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron® ESd 480 PEEK, static dissipative, (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® ESd 520HR (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® ESd 420 V (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® MPR-1000 (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® CMP LL5 Polyester (ASTM Product Data Sheet)

P1SM34e / 89258

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.