MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Pyro-Log Fiber and Pyro Packaging R Grade Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Pyro-Log is an uncompressed monolithic mass of ceramic fiber. Pyro-Log fiber is available in 6" and 8" (152 mm and 203 mm) thicknesses with densities up to 15 pcf (240 kg/m3 ). Manufactured in three ceramic fiber grades, R, ZR and C, the Pyro-Log fiber can be used in a wide range of applications. Pyro-Log fiber is the basic building block for all Pyro-Bloc applications. All Pyro-Log fiber is produced with a special lubricant that allows the fibers to be intensely needled to attain densities up to 15 pcf. This lubricant also adds pliability which allows true multi-directional compression during installation. At moderate temperatures this lubricant burns out and the fiber mass becomes rigid. This feature, unique to Pyro-Log fiber, assists during installation and provides the durability and toughness necessary for long life.

Applications:

  • Low mass kiln cars
  • Fired heater floors
  • Back up insulation for insulating firebrick and castable lining
  • Fill gaps or small spaces where standard shapes are not practical

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.128 g/cc
 0.160 g/cc
 0.192 g/cc
 0.240 g/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0700 W/m-K
@Temperature 260 °C
at 160kg/m3; ASTM C201
 0.150 W/m-K
@Temperature 538 °C
at 160kg/m3; ASTM C201
 0.260 W/m-K
@Temperature 816 °C
at 160kg/m3; ASTM C201
 0.390 W/m-K
@Temperature 1093 °C
at 160kg/m3; ASTM C201
Melting Point 1760 °C
Maximum Service Temperature, Air 1204 °CContinuous Use
 
Component Elements PropertiesOriginal ValueComments
Al2O3 47 %
SiO2 53 %
 
Descriptive Properties
Classification Temperature (°C)1316
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool 80 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 3000 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber

CMORF70154 / 203452

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.