MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-ABS 3365 High Impact ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Data provided by Multibase.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792-91
Linear Mold Shrinkage 0.0050 cm/cmASTM D955-89
Melt Flow 5.0 g/10 min(Condition G) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ASTM D785-95
Tensile Strength, Ultimate 39.3 MPaASTM D638-95
Elongation at Break 50 %ASTM D638-95
Flexural Modulus 2.276 GPaRT; ASTM D-790-95
Izod Impact, Notched 3.20 J/cmASTM D256-93a
Gardner Impact 31.1 JASTM D5420-93
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 175 °Cinjection molded unannealed; ASTM D-648-95
 220 °Cinjection molded annealed; ASTM D-648-95
 220 °Ccompression molded annealed; ASTM D-648-95
Vicat Softening Point 94.0 °CASTM D1525-95
Flammability, UL94 HB
@Thickness 1.59 mm
 HB
@Thickness 3.17 mm
 
Optical PropertiesOriginal ValueComments
Gloss 85 - 90 %ASTM D2457-90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Supreme Petrochem SC 6501 Toughened Polystyrene
Supreme Petrochem SP 256 Toughened Polystyrene
Dow AIM® 4810 High Impact Styrenic Resin
Dow AIM® 4800 High Impact Styrenic Resin
Americas Styrenics Styron® 482 High Impact Polystyrene

PLA295 / 49692

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.