MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Okulen® OKULEN® 2000 – MD – FN5790 UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: OKULEN® 2000 – MD – FN5790 is a “Metal Detectable” UHMW-PE Polymer compound with a molecular weight of approx 9 mio. g/mol. The material has a very good wear resistance, a low coefficient of friction and a high impact strength. Responsibility to review the detection rate is up to the end user.

Properties: Metal detectable; Good sliding properties; Very good abrasion resistance; Excellent chemical resistance; Good impact strength; EU 1935/2004 & 10/2011 – conform

Color: Azure blue FN5790/similar RAL5009

Range of applications: Food industry; Conveying industry

Information provided by Okulen

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 1.05 g/cc>= 0.0379 lb/in³DIN EN ISO 11831-1
Water Absorption <= 0.10 %<= 0.10 %DIN EN ISO 62
Molecular Weight 9.00e+6 g/mol9.00e+6 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 66
@Time 3.00 sec
66
@Time 0.000833 hour
6 mm plate; DIN EN ISO 868
Tensile Strength, Yield >= 17.0 MPa>= 2470 psi1B- 50 mm/min; DIN EN ISO 527-2
Elongation at Break >= 200 %>= 200 %1B- 50 mm/min; DIN EN ISO 527-2
Tensile Modulus >= 0.650 GPa>= 94.3 ksi1B- 1 mm/min; DIN EN ISO 527-2
Izod Impact, Notched (ISO) >= 100 kJ/m²>= 47.6 ft-lb/in²DIN EN ISO 21304-2
Coefficient of Friction, Dynamic 0.180.18ASTM D1894
Coefficient of Friction, Static 0.200.20ASTM D1894
Abrasion 9090Sand-Slurry; DIN EN ISO 15527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
8.33 - 11.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
Thermal Conductivity 0.410 W/m-K2.85 BTU-in/hr-ft²-°F
Melting Point 135 - 137 °C275 - 279 °FDIN EN ISO 11357-1
Flammability, UL94 HBHB
 
Descriptive Properties
Operation Temperature80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POKUL1035 / 307312

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.