MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chevron Phillips MC3500 General Purpose Crystal Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Description

Chevron polystyrene resin MC3500 is a general purpose, injection molding thermoplastic compound combining moldability with fast set-up and excellent mold release. It has a low bulk factor and good electrical, mechanical and optical properties. Chevron MC3500 crystal complies with Food Additive Regulation 21CFR177.1640 for polystyrene, which states that such materials may be safely used in contact with foods.

Applications

Chevron MC3500 is widely used for injection molding of toys, thin- and heavy-walled containers, appliance parts, housewares and medical applications.Information provided by Chevron Phillips Chemical Company.

The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Melt Flow 9.0 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7200 psiat 2.0 in/min; ASTM D638
Tensile Strength, Yield 7200 psiat 2.0 in/min; ASTM D638
Elongation at Break 3.0 %ASTM D638
Tensile Modulus 450000 psiASTM D638
Flexural Strength 10000 psiASTM D790B
Flexural Modulus 460000 psiASTM D790B
Izod Impact, Notched 0.250 ft-lb/in1/4 in.; ASTM D256
 0.350 ft-lb/in1/8 in.; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 186 °FASTM D648
Vicat Softening Point 215 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Supreme Petrochem SC 206 General Purpose Polystyrene
NIZHNEKAMSKNEFTEKHIM 525 General Purpose Polystyrene
NIZHNEKAMSKNEFTEKHIM 524B General Purpose Polystyrene
M. Holland Company GS411 Polystyrene
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance

PPSRA20 / 58250

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.