MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sandvik Creusabro Dual Plate and sheet
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Creusabro Dual is a new, advanced, high performance grade of abrasion resistant steel dedicated to severe impact and sliding wear conditions in service. Thanks to its outstanding wear resistance, the use of Creusabro Dual should be considered in applications where conventional water quenched steels (500 HB, 550 HB), hard faced plates, or cast wear parts are traditionally used. Creusabro Dual advanced properties have been created using an innovative metallurgical concept, based on a unique combination of chemical composition and heat treatment procedures (oil quenching), which reduces the level of residual stresses encountered with drastic quenching methods such as water. This confers to Creusabro Dual an outstanding extra wear resistance, a strong resistance in extreme impact and sliding conditions and a very efficient work hardening capability in service. No other steel offers such high wear and abrasion resistance at this level of hardness (500HB), combined with high resistance to cracking in service.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 480
Tensile Strength, Ultimate 1630 MPa
 900 MPa
@Temperature 500 °C
 1250 MPa
@Temperature 400 °C
 1650 MPa
@Temperature 200 °C
Tensile Strength, Yield 1200 MPa
@Strain 0.2 %
 520 MPa
@Strain 0.2 %,
Temperature 500 °C
 880 MPa
@Strain 0.2 %,
Temperature 400 °C
 1080 MPa
@Strain 0.2 %,
Temperature 200 °C
Elongation at Break 10 %
Modulus of Elasticity 205 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 - 100 °C
 12.0 µm/m-°C
@Temperature 20.0 - 200 °C
 12.5 µm/m-°C
@Temperature 20.0 - 300 °C
 13.0 µm/m-°C
@Temperature 20.0 - 400 °C
 14.0 µm/m-°C
@Temperature 20.0 - 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.40 %
Chromium, Cr 0.70 %
Manganese, Mn <= 1.3 %
Molybdenum, Mo <= 0.34 %
Nickel, Ni 0.45 %
Sulfur, S <= 0.0020 %
Titanium, Ti <= 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Creusabro 4800 Plate and sheet
Industeel CREUSABRO® 4000 High Wear Resistant Steel
AISI 4320 Steel, single quenched and tempered (carburized 925°C (1700°F) for 8hrs, pot cooled, reheated to 815°C (1500°F), quenched in agitated oil, 230°C (450°F) temper), 1.9 mm case depth
AISI 1045 Steel, Quenched and Tempered to 450 HB
202 Stainless Steel, 50% cold reduced sheet, longitudinal orientation

NSANDV5049 / 199613

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.