MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
Saint-Gobain Meldin® 5530 Polyketone
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: This grade has been specially created for parts submitted to tribological stresses. At high PV, wear and friction are very low and this is very important to increase the lifetime of the different components.

Having a high tensile, compressive and flexural strength, Meldin® 5000 materials are injection molded into tight-tolerance finished components in simple or complex designs that can exhibit metal-like finishes without expensive machining or secondary operations, and with the advantages of being lighter and corrosion resistant.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 49.0 MPa
@Temperature 249 °C
ASTM D638
 170 MPa
@Temperature 23.0 °C
ASTM D638
Elongation at Break 1.9 %ASTM D638
Tensile Modulus 18.0 GPaASTM D638
Flexural Strength 45.0 MPa
@Temperature 249 °C
ASTM D790
 240 MPa
@Temperature 23.0 °C
ASTM D790
Flexural Modulus 17.0 GPaASTM D790
Compressive Strength 35.0 MPa
@Temperature 200 °C
ASTM D695
 176 MPa
@Temperature 23.0 °C
ASTM D695
Izod Impact, Notched 70.0 J/m
Izod Impact, Unnotched 430 J/m
Coefficient of Friction, Dynamic 0.050 - 0.070Dry; ASTM D3702
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 - 143 °C
Average; Below Tg; ASTM E831
 90.0 µm/m-°C
@Temperature >=143 °C
Average; Above Tg; ASTM E831
CTE, linear, Parallel to Flow 12.0 µm/m-°C
@Temperature 20.0 - 143 °C
Below Tg; ASTM E831
 12.0 µm/m-°C
@Temperature >=143 °C
Above Tg; ASTM E831
Thermal Conductivity 1.30 W/m-KASTM F433
Melting Point 343 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 330 °CASTM D648
Glass Transition Temp, Tg 143 °CASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTGQ996i / 305355

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.