System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC XENOY™ X5630Q PC+PBT (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Material Notes:
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.35
g/cc
ISO 1183
Water Absorption
0.42 %
23°C/sat; ISO 62
Moisture Absorption
0.140 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0050
-
0.0070
cm/cm
SABIC method
Melt Flow
16
g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
20
g/10 min
@Load 5.00 kg,
Temperature 265 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
50.0
MPa
5 mm/min; ISO 527
Tensile Strength, Yield
56.0
MPa
5 mm/min; ISO 527
Elongation at Break
8.0 %
5 mm/min; ISO 527
Elongation at Yield
3.3 %
5 mm/min; ISO 527
Tensile Modulus
4200
MPa
1mm/min; ISO 527
Flexural Yield Strength
92.0
MPa
2 mm/min; ISO 178
Flexural Modulus
4100
MPa
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
7.00
kJ/m²
80*10*4; ISO 180/1A
5.00
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
100
kJ/m²
80*10*4; ISO 180/1U
80.0
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact, Notched
8.00
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
52.0
µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
72.0
µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi)
110
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point
137
°C
Rate B/50; ISO 306
140
°C
Rate B/120; ISO 306
Processing Properties
Original Value
Comments
Processing Temperature
60.0
-
80.0
°C
Hopper Temperature
Nozzle Temperature
260
-
275
°C
Injection Molding
Zone 1
240
-
270
°C
Zone 2
250
-
275
°C
Zone 3
260
-
280
°C
Melt Temperature
265
-
275
°C
Mold Temperature
60.0
-
100
°C
Drying Temperature
110
-
120
°C
Injection Molding
Dry Time
4.00
-
6.00
hour
Injection Molding
Moisture Content
0.020 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABI10872 / 244339
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.