Hostacom TRC 333N TABAK is a high flow thermoplastic olefin elastomeric (TPO) with excellent scratch resistance, very low stress whitening and low emissions and good stiffness/impact balance. It is typically used for interior trim applications. Applications: Automotive Parts, Interior Automotive ApplicationsInformation provided by LyondellBasell. |