MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Avient Edgetek® XP9242701 Polyphenylene Sulfide (PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 sec

Information provided by PolyOne

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 g/ccASTM D792
Filler Content 10 %Carbon Fiber Reinforcement
 30 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 258 MPaASTM D638
Flexural Modulus 18000 MPaASTM D790
Charpy Impact, Notched 60.0 J/cm²J/m; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 1.00e+9 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 265 °CUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 270 - 280 °C
Middle Barrel Temperature 290 - 330 °C
Front Barrel Temperature 290 - 330 °C
Nozzle Temperature 280 - 320 °C
Mold Temperature 120 - 150 °C
Drying Temperature 130 - 150 °C
Dry Time 4.00 - 6.00 hour
Injection Pressure 70.0 - 100 MPa
Hold Pressure 50.0 - 80.0 MPa
Back Pressure 1.00 - 2.50 MPa
Screw Speed 80 - 120 rpm
 
Descriptive Properties
FormsPellets
Generic MaterialPPS
Generic NamePolyphenylene Sulfide (PPS)
Processing MethodInjection Molding
Regional AvailabilityAsia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® CP-0301 Fiber Compound
Mocom (ALBIS) Tedur® L 9200-1 Polyphenylene Sulfide
Evonik PROCON™ PPS Polyphenylene Sulfide
DuPont Mobility and Materials VESPEL TP-8474 Polyimide
Celanese Fortron® 4184 L6 Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

PH0POL1312 / 145881

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.