MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Argo-braze™ 72V Silver Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Argo-braze™ 72V is a silver-copper brazing filler metal with a eutectic composition, and has a melting point of 778°C unlike most other brazing filler metals that have a melting range.

It is manufactured to meet vacuum tube grade requirements with low and controlled levels of volatile impurities. Consequently it can be used on vacuum tube devices that operate at moderate temperatures and where volatile elements might be detrimental to the performance of the component.

Having a single melting temperature of 778°C makes the alloy very free flowing and able to penetrate narrow joint gaps. On silver and copper parent materials the flow of the alloy is reduced and the re-melt temperature is increased due to the filler metal taking silver or copper into solution when molten. Exercising careful control of the brazing cycle brazing temperatures and time at temperature can reduce this effect.

Argo-braze™ 72V shows only limited wetting on iron and nickel base metals and on cemented tungsten carbides.

Where ceramics are being brazed to a low expansion nickel alloy, care should be taken (nickel plating / stress relieving) to prevent intergranular penetration (liquid metal stress cracking) of the nickel alloy.

Argo-braze™ 72V is standardly supplied as EN 1044 vacuum grade V1, but it can also be supplied in the vacuum grade V2, both of which are suitable for vacuum tube applications. The alloy can also be supplied as the nonvacuum tube grade material EN 1044 AG401.

Argo-braze™ 72V was formerly known as Silver-Copper Eutectic™.

Argo-braze™ 72V is used for brazing silver, copper and nickel based alloys as well as metalized ceramics. Typical applications include components for vacuum tube devices.

This product can be used to braze in hydrogen, an inert atmosphere or in a vacuum without the need for a flux. When vacuum brazing a partial pressure brazing technique should be used to prevent the vaporization of the silver within the alloy.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 778 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 28 %
Silver, Ag 72 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey Argo-braze™ 502 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 56 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 60 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 60V Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 61V Silver Brazing Filler Metal

NJMMJ9715 / 186116

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.