MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Crucible Steel S7 XL (Premium AISI S7) Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Crucible S7XL is a double refined, high purity grade of S7. The remelt operation produces a cleaner steel with a more uniform microstructure, offering the following advantages over conventional S7:
  • Better Consistency in Wire EDM Cutting
  • Higher Polishability for Critical Finish Plastic Molds
  • More Uniform Texturing for Plastic Molds
  • Higher Transverse Impact Toughness (Across the Grain) Crucible S7 XL can be used in any application where AISI S7 is used.

    Information provided by Crucible Specialty Metals.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 7.83 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Brinell 187 - 220Annealed
    Hardness, Rockwell C 57Austenitizing Temperature- 955°C
    Modulus of Elasticity 207 GPa
    Charpy Impact 125 JAustenitizing Temperature- 955°C
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 12.6 µm/m-°C
    @Temperature 20.0 - 205 °C
     13.7 µm/m-°C
    @Temperature 20.0 - 540 °C
    Thermal Conductivity 28.5 W/m-K
    @Temperature 95.0 °C
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C 0.55 %
    Chromium, Cr 3.25 %
    Iron, Fe 93.5 %As Remainder
    Manganese, Mn 0.70 %
    Molybdenum, Mo 1.4 %
    Silicon, Si 0.35 %
    Vanadium, V 0.25 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Carpenter S7 Alloy Tool Steel (AISI S7)
    Crucible Steel S7 (AISI S7) Tool Steel
    EDRO #7 Shock Resistant S7 Tool Steel
    Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
    Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)

    NCRUC025 / 16018

    Specialty Compounds RTP Company

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.