MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arya Sasol HEX4460 PE80+ High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HEX4460 PE80+ is a high molecular weight, high density polyethylene (HDPE) with high melt viscosity for extrusion. This grade, which is produced by 1-hexene co-monomer, is classified as PE 80+ and provides excellent stress crack resistance properties (ESCR) combined with very good long-term hydrostatic strength and good processability. Typical customer applications are underfloor heating and multilayer pipe for heating and plumbing. HEX4460 PE80+ has been manufactured under Basell license.

Application: Drinking water pipe, drainage pipe, plumbing, heating & cooling

Forms: Pellets

Attribute: Good Resistance to SCG & RCP; Good Processability; Outstanding ESCR; Good Creep Strength; Good Chemical Resistance; Very Good Low Temp. Impact Resistance

Additives: Antioxidant: Yes; Processing Aid: No; Antiblock: No; Slip Agent: No

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.944 g/ccISO 1183
Environmental Stress Crack Resistance >= 150 hour
@Pressure 3.50 MPa,
Temperature 80.0 °C
FNCT, 2% Arkopal N100; ISO 16770
ESCR 10% Igepal® >= 1000 hourMethod B; ASTM D1693
Oxidative Induction Time (OIT) >= 30 min
@Temperature 200 °C
ISO 11357
Melt Flow 0.33 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 6.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaISO 527-1, -2
Tensile Strength, Yield 25.0 MPaISO 527-1, -2
Elongation at Break >= 1000 %ISO 527-1, -2
Elongation at Yield 11 %ISO 527-1, -2
Modulus of Elasticity 0.700 GPaISO 527-1, -2
1% Secant Modulus >= 1000 MPaFlexural Modulus; ASTM D790
Izod Impact, Notched (ISO) 26.0 kJ/m²ISO 180 A
Tensile Impact Strength 167 kJ/m²
@Temperature -30.0 °C
Notched, Type 1, Method A; ISO 8256
 
Thermal PropertiesOriginal ValueComments
Melting Point 129 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75
Vicat Softening Point 126 °C
@Load 1.02 kg
Method A; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 230 °CExtruder temperature profile
Melt Temperature 205 - 240 °C
 
Descriptive Properties
Hydrostatic Pressure Test>100 hrs9.0 MPa @ 20°C, ISO 1167
 >1000 hrs4.0 MPa @ 80°C, ISO 1167
Minimum Required Strength>8 MPaISO 12162
Resistance to Rapid Crack Propagation>6 barPc @ 0°C
Resistance to Slow Crack Growth>1000 hrs4.6 MPa @ 80°C, ISO 13479

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARYA017 / 250471

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.