MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Total 6480 High Density Polyethylene, Clarity Cast Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Polyethylene: Clarity High Density Cast Film Resin

Characteristics:

  • High stiffness
  • High clarity
  • Excellent surface gloss
  • High tensile strength
  • Good barrier properties
  • Low gel content

Applications:

  • Overwrap
  • Food packaging
  • Coextrusion
  • Extrusion coating

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.962 g/ccASTM D792
Water Vapor Transmission 0.220 g/100 in²/day
@Temperature 37.8 °C
ASTM E96/66
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5000 psifilm; ASTM D882
Elongation at Break 1000 %ASTM D882
Secant Modulus 95.0 ksiASTM D882
Elmendorf Tear Strength MD 35 gASTM D1922
Elmendorf Tear Strength TD 50 gASTM D1922
Dart Drop Test 85.0 gASTM D1709
 
Thermal PropertiesOriginal ValueComments
Melting Point 265 °FASTM D3417
 
Optical PropertiesOriginal ValueComments
Haze 15 %ASTM D1003
Gloss 65 %ASTM D523
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Melt Temperature 450 - 500 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reliance Industries Relene E52009 Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Formosa Plastics Formolene® LH5204 Injection Molding HDPE
ExxonMobil Hicor® 90 BIHD-M OHD Film
Daikin NEOFLON® AP-201 PFA

PTOTAL753 / 130478

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.