PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PC/ABS 1420 has excellent mechanical properties and is easy to extrude. Typical applications include extruded sheets for thermoforming of trays for the electronics industry when good rigidity is needed. Information provided by Premix Thermoplastics Inc. |