Hostacom TRC 1193N NATURAL is high melt flow, 1,900 MPa flexural modulus, low density thermoplastic polyolefin (TPO) resin. It has an excellent balance of processability, rigidity, impact, scratch and mar resistance. It is typically used for injection molding of Instrumental Panels and other interior trim parts or components with good surface appearance properties. Applications: Instrument Panels, Interior Automotive ApplicationsInformation provided by LyondellBasell. |