MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow R7021-50RNA Polypropylene Random Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded; Polypropylene, Molded

Material Notes: DOW™ R7021-50RNA Polypropylene Resin is a random copolymer designed for thin wall injection molding applications desiring high clarity.

    Main Characteristics
  • Good impact properties
  • Excellent optics
  • Fast cycle times
  • Contains clarifier and antistat additives
  • Complies with U.S. FDA 21 CFR 177.1520 (c)3.1a

Former Dow grade acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Index of Compound 50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27.6 MPaASTM D638
Elongation at Yield 11 %ASTM D638
Flexural Modulus, 1% Secant 1070 MPaASTM D790A
Izod Impact, Notched 53.4 J/mASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °CUnannealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %
@Thickness 0.508 mm
ASTM D1003
 14 %
@Thickness 1.02 mm
ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorPURE™ RJ377MO Polypropylene, Transparent Random Copolymer
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade
Dow 5E16S Polypropylene Homopolymer Resin
Dow R792-35RNA Polypropylene Random Copolymer Resin

PDOW0983 / 93319

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.