MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Celanese Micromax™ 2140 Paste for Resistor Applications
Material Notes: Resistor Composition For Hybrid Circuits

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Drying Temperature 150 °C
Dry Time 0.167 hour
Shelf Life 6.00 Month
@Temperature <=25.0 °C
unopened containers, from date of shipment
 
Descriptive Properties
Blend member or series2100srs
Cold Temperature Coefficient Resistance-50 to 50from +25 to 0°C for cold TCR
Electrostatic discharge<0.1Untrimmed resistors, 0.8mm x 0.8mm @ 5kV
 <8Untrimmed resistors, 0.8mm x 0.8mm @ 25kV
Hot Temperature Coefficient Resistance-50 to 50from +25 to +70 for hot TCR
Leveling time5 to 10
Mask emulsion (µm)5 to 10
Mask mesh325Screen Type: Stainless steel
Noise (Max dB)-11Quan-Tech model 315C, Untrimmed resistors, 0.8mm x 0.8mm.
PolymerPaste
Solvent or thinnerMicromax™ 8250
Temperature Coefficient Resistance, firing sensitivity<0.5 ppm/°C/°C.The effect of firing temperature on TCRs between 825 and 875°C
Temperature Coefficient Resistance, length effect<40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDTF9309zj / 296010

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.