MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Pressure Seal 14701 Chlorosulfonated
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 14701 is a 70 durometer black colored general purpose Hypalonelastomer. It exhibits good low temperature flexibility.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 CE 725 F19; 3 CE 725 F19

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68
 44
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #3
 68
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 72
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1
 72
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 72
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 76
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 76
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
Tensile Strength 2849 psi
 1743.6 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 1743.6 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 1760.7 psi
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #3
 3105.4 psi
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1
 3105.4 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 3105.4 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 310 %
 129.9 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged
 129.9 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 249.9 %
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #3
 260.1 %
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1
 260.1 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 260.1 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged
100% Modulus 438 psi
Tear Strength 147 pliDie B
 200 pliDie C
Compression Set 7.9 %
@Temperature 23.0 °C,
Time 79200 sec
Plied
 8.3 %
@Temperature 23.0 °C,
Time 79200 sec
Solid
 76.4 %
@Temperature 125 °C,
Time 79200 sec
Solid
 81.4 %
@Temperature 125 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -87.0 °F
Shrinkage 4.1 %
@Temperature 100 °C,
Time 252000 sec
Volume, ASTM Oil #1
 13.5 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 71.2 %
@Temperature 100 °C,
Time 252000 sec
Volume, ASTM Oil #3
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL092 / 318302

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.