MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sandvik 19.12.3.LSi Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.12.3.Nb is a niobium stabilized filler metal suitable for joining stainless steels of the 18Cr/8Ni/Mo, 18Cr/8Ni/Mo/Ti and 18Cr/8Ni/Mo/Nb types. Due to the strengthening effect of niobium, this grade is recommended if the weld metal will be exposed to temperatures above 400°C (750 F).

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 160
Tensile Strength, Ultimate 440 MPa
@Temperature 400 °C
 610 MPa
@Temperature 20.0 °C
Tensile Strength, Yield 290 MPa
@Strain 0.2 %,
Temperature 400 °C
 400 MPa
@Strain 0.2 %,
Temperature 20.0 °C
Elongation at Break 29 %
@Temperature 400 °C
 37 %
@Temperature 20.0 °C
Reduction of Area 68 %
Charpy Impact 50.0 J
@Temperature -196 °C
 130 J
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
 16.0 W/m-K
@Temperature 100 °C
 19.0 W/m-K
@Temperature 300 °C
 21.0 W/m-K
@Temperature 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %All Weld Metal
 <= 0.025 %AIM
 <= 0.025 %Nominal
Chromium, Cr 18.3 %Nominal
 18.5 %All Weld Metal
 18.5 %AIM
Manganese, Mn 1.7 %All Weld Metal
 1.8 %AIM
 1.8 %Nominal
Molybdenum, Mo 2.6 %AIM
 2.6 %Nominal
 2.6 %All Weld Metal
Nickel, Ni 11.5 %All Weld Metal
 12 %AIM
 12.3 %Nominal
Nitrogen, N 0.050 %Nominal
 0.060 %All Weld Metal
 <= 0.060 %AIM
Phosphorus, P 0.010 %All Weld Metal
 <= 0.025 %AIM
 <= 0.025 %Nominal
Silicon, Si 0.90 %AIM
 0.90 %Nominal
 0.90 %All Weld Metal
Sulfur, S 0.013 %All Weld Metal
 <= 0.015 %AIM
 <= 0.015 %Nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5087 / 199651

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.