MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LyondellBasell Hostacom HKC 1339T BLACK Polypropylene with 20% Talc Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Hostacom HKC 1339T BLACK is a 20% talc filled polypropylene homopolymer that is available in pellet form. This resin is typically used in injection molding applications. Applications: Automotive Parts

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/cc
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 37.0 MPa
Elongation at Yield 5.3 %
Flexural Modulus 3100 MPa2mm/min, chord
Charpy Impact, Notched 2.40 kJ/m²
@Temperature -30.0 °C
 4.00 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °Cunannealed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYFORT™ FPP 1607 Talc Filled Homopolymer Polypropylene
Avient Maxxam™ DP-8928-2-1000 Polypropylene
Avient Maxxam™ PPR-20G Black Polypropylene Homopolymer (PP Homopolymer)
LyondellBasell Hostacom HKG 339N BLACK Polypropylene, Glass/Mineral Reinforced
LyondellBasell Hostacom GP621-2 NAT Polypropylene with 10% Talc Filler

PEQT7968 / 219605

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.