PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® TPE 1503 has retained the excellent mechanical properties of the base elastomer. Typical applications included extruded profiles, sheets and injection moulded technical parts. Processing: PRE-ELEC® TPE 1503 compound can be extruded or injection moulded in the machines using normal processing conditions as with TPE. Test Specimen: 10[mm] wide moulded rod Information from Premix OY |