Grade H12G-01 is a general purpose homopolymer. This material meets the requirements of the US Food and Drug Administration as specified in 21 CFR 177.1520 for use in food-contact applications for food type Categories I through IX of Table 1, under conditions of use A through H of Table 2 in Title 21 CFR, Part 176.170(c).Applications:- General Purpose Injection and Extrusion
- Housewares
- Rigid Packaging
- Caps & Closures
- Film and SheetInformation provided by Ineos Olefins & Polymers USA
|