MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC VALOX™ FR 310SE0 PBT (Asia)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX 310SE0 is an unreinforced, flame retardant Polybutylene Terephthalate (PBT) injection moldable grade with excellent chemical resistance. It has a UL94V0@0.71mm and 5VA@3.0mm flame rating. This is a good candidate for thin wall applications in the electrical industry including bobbins, keyboards, switches and appliance housings.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
 1.40 g/ccASTM D792
Density 1.40 g/ccISO 1183
Water Absorption 0.36 %23°C/sat; ISO 62
Moisture Absorption 0.0800 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.011 - 0.018 cm/cmSABIC method
 0.0090 - 0.016 cm/cm
@Thickness 0.750 - 2.30 mm
SABIC method
 0.015 - 0.023 cm/cm
@Thickness 2.30 - 4.60 mm
SABIC method
 0.015 - 0.023 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0090 - 0.019 cm/cmSABIC method
 0.010 - 0.017 cm/cm
@Thickness 0.750 - 2.30 mm
SABIC method
 0.016 - 0.024 cm/cm
@Thickness 2.30 - 4.60 mm
SABIC method
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 8.6 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ISO 2039-2
Ball Indentation Hardness 105 MPaISO 2039-1
Tensile Strength at Break 40.0 MPa50 mm/min; ISO 527
 52.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa50 mm/min; ISO 527
 58.0 MPa50 mm/min; ASTM D638
Elongation at Break 18 %50 mm/min; ASTM D638
 18 %50 mm/min; ISO 527
Elongation at Yield 5.0 %50 mm/min; ISO 527
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2800 MPa1mm/min; ISO 527
 2820 MPa5 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 101 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2600 MPa2 mm/min; ISO 178
 2620 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 40.0 J/mASTM D256
 25.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²ISO 179/2C
 8.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 200 JASTM D3763
Taber Abrasion, mg/1000 Cycles 19CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 18.0 kV/mm
@Thickness 1.00 mm
shorttime; IEC 60243-1
 18.4 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
 24.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0020
@Frequency 100 Hz
IEC 60250
 0.0125
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 0.00 - 60 secUL 746A
 60 - 120 secASTM D495
Comparative Tracking Index 100 VIEC 60112
 175 VIEC 60112
 175 - 250 VUL 746A
Hot Wire Ignition, HWI 30 - 60 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 79.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
 131 µm/m-°C
@Temperature 60.0 - 138 °C
ASTM E831
CTE, linear, Transverse to Flow 73.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 79.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.240 W/m-KISO 8302
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 150 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 162 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 73.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 71.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
 74.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 170 °CRate B/120; ISO 306
 170 °CRate B/50; ASTM D1525
 170 °CRate B/50; ISO 306
 212 °CRate A/50; ISO 306
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 120 °CUL 746B
UL RTI, Mechanical without Impact 140 °CUL 746B
Flammability, UL94 V-0
@Thickness 0.710 mm
UL 94
 5VA
@Thickness 3.00 mm
UL 94
Oxygen Index 30 %ISO 4589
Glow Wire Test 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 255 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 255 °C
Zone 3 245 - 260 °C
Melt Temperature 245 - 260 °C
Mold Temperature 50.0 - 75.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00130 - 0.00250 cm
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10335 / 243802

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.