MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Cabot CABELEC® CA6748 PP, Conductive Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product highlights: CABELEC CA6748 conductive compound is a static dissipative compound made from carbon black dispersed in a polypropylene copolymer. Its electrical and mechanical properties are not dependent on atmospheric conditions. It has good rigidity and can be easily processed on conventional molding equipment.

Key applications: The static dissipative nature of CABELEC CA6748 conductive compound provides products with a higher resistivity than typical conductive materials and can provide long-lasting static dissipation. Typical areas of applications are electronics packaging, ammunition works, mines, petroleum plants, and other environments where it is important to mitigate the hazard of electrostatic discharge.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Melt Flow 3.7 g/10 min
@Load 230 kg,
Temperature 2.16 °C
ISO 1133
 22 g/10 min
@Load 230 kg,
Temperature 5.00 °C
ISO 1133
 86 g/10 min
@Load 230 kg,
Temperature 10.0 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64
@Time 15.0 sec
ISO 868
Tensile Strength at Break 16.0 MPaISO 527
Tensile Strength, Yield 22.0 MPaISO 527
Elongation at Break 130 %ISO 527
Flexural Modulus 1290 MPaISO 178
Izod Impact, Notched (ISO) 44.0 kJ/m²ISO 180A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.00e+6 ohm-cmIEC 61340-2-3
Surface Resistance <= 1.00e+8 ohmIEC 61340-2-3
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75
Vicat Softening Point 148 °C
@Load 1.02 kg
ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °Cbarrel
Nozzle Temperature 220 °C
Mold Temperature 30.0 °C
Drying Temperature 90.0 °C
Dry Time 2.00 - 3.00 hour
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT055 / 315790

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.