MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa DANCOLL® 254-63 Polyether based polyurethane prepolymer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: DANCOLL® 254-63 is a polyether based polyurethane prepolymer with blocked isocyanate. This solvent-based prepolymer is mainly used as basic raw material for flock adhesives and laminating adhesives.

Application: DANCOLL® 254-63 is a optimum basic raw material for the production of flock adhesives. It are mainly flocked EPDM, SBR and other rubber profiles by means of polyester- and polyamide flock. For the crosslinking and achieving of the application viscosity the product must be crosslinked with a corresponding DANCURE crosslinker. Suggested formulation for classic flock adhesives DANCOLL® 254-63 78,0 weights by part DANCURE® 120 62,0 weights by part After the blending of both components the pot life of the blend will be 2-3 days at room temperature. The crosslinking of the blend occurs at 150°C in a time period of 2,5 minutes. The higher the temperature the faster the crosslinking will occur. By adjustment of the temperature and speed at the pass through the drying cabinet (crosslinking oven) the desired reaction can be chosen.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 61 - 65 %DIN 53.189
Brookfield Viscosity 80 - 100 cPRVT
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AspectBeige liquid
SolventMEK, ethyl acetate, tolyole

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ032 / 294452

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.