MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 5 Polydimethylsiloxanic Fluids
Categories: Fluid

Material Notes: Description: BLUESIL FLD 47 V 3 to 47 V 20 are a low viscosity polydimethylsiloxanic fluids.

Applications: BLUESIL FLD 47 V 3 to 47 V 20 are used as:

  • Lubricants (to lubricate elastomers or plastics on metal).
  • Low temperature hydraulic fluids.
  • Dielectric fluids (impregnating paper for capacitors).
  • Thinning agents for BLUESIL RTV (two component, room temperature vulcanizing silicone elastomers).
Advantages:
  • Very good heat stability
  • Good dielectric properties
  • Low surface tension
  • High compressibility
  • Excellent weathering resistance
  • Good oxidation resistance
  • Low freezing point
  • Less change in viscosity as a function of temperature than non silicone oils
  • Good resistance to high and prolonged shear forces
  • Low heat of combustion
  • Limited combustion.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/cc
Kinematic Viscosity 5.0 cSt
Surface Tension 19.7 dynes/cm
Storage Temperature -20.0 - 30.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.10e+15 ohm-cm
Dielectric Constant 2.6
@Frequency 500 - 100000 Hz
Dielectric Strength 356 V/mil
Dissipation Factor 0.000011
@Frequency 100000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 25.0 - 100 °C
Thermal Conductivity 0.120 W/m-K
Melting Point -65.0 °C
Flash Point 120 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.397
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.0 Month
 
Descriptive Properties
AppearanceColorless limpid liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 3 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 41V0.65 Fluid
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 100 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 50 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 100 Polydimethylsiloxane Fluid

PBLUST099 / 191075

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.