MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes:

Characteristics:

  • Outstanding Chemical Resistance
  • Outstanding Wear Resistance
  • Outstanding Resistance to Hydrolysis
  • Excellent Mechanical Properties
  • Outstanding Thermal properties
  • Very good Dielectric Strength, Volume Resistivity, Tracking Resistance
  • Excellent Radiation Resistance

Applications:

  • Medical appliances including implantation
  • Aerospace application
  • Engineering applications like compressor plates, valve seats, moving parts for textile machines
  • Electrical and communication cables
  • Scientific laboratory instruments


Information provided by Gharda Chemicals

Solvay Advanced Polymers completed its acquisition of this product line in May 2006.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Filler Content 30 %
Water Absorption 0.080 %24 Hours; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 102ASTM D785
Tensile Strength, Yield 160 MPaASTM D638
Elongation at Break 2.5 %ASTM D638
Tensile Modulus 10.0 GPaASTM D638
Flexural Strength 260 MPaASTM D790
Flexural Modulus 10.0 GPaASTM D790
Izod Impact, Notched 95.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohmASTM D257
Dielectric Constant 2.9
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mmASTM D149
Dissipation Factor 0.0030
@Frequency 60 Hz
ASTM D150
Comparative Tracking Index 150 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Maximum Service Temperature, Air 260 °CContinuous Use; UL-746B
Deflection Temperature at 1.8 MPa (264 psi) 315 °CASTM D648
Glass Transition Temp, Tg 148 °CASTM D3482
Flammability, UL94 V-0
@Thickness 0.800 mm
UL 94
Oxygen Index 45 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Renol PEEKSP0002 Polyetheretherketone, 30% Glass Fiber
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Solvay APC-2/S-2 Glass PEEK with Glass Fiber Reinforced Unidirectional Tape
DuPont Mobility and Materials Crastin® SK615SF NC010 PBT-GF30

PGHARDA24 / 41797

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.