MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zell-Metall Engineering Plastics Zellamid 1100 MO
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, MoS2 Filled

Material Notes: Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.

Color: black

Applications: For conveyor screws

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cc
Moisture Absorption at Equilibrium 2.5 - 3.0 %50% RH
Water Absorption at Saturation 6.0 - 7.0 %23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83 - 85DIN 53505
Ball Indentation Hardness 165 MPaDIN 53456
Tensile Strength at Break 90.0 - 92.0 MPaDIN 53455
Elongation at Break 10 - 30 %DIN 53455
Tensile Modulus 4.10 GPaDIN 53457
 0.900 GPa
@Temperature 100 °C
DIN 53457
Charpy Impact Unnotched NBDIN 53453
Charpy Impact, Notched 2.20 - 2.80 J/cm²DIN 53453
Coefficient of Friction 0.050 - 0.10to steel, added lubrication
 0.30 - 0.35to steel, no lubrication; ISO/DTR 7147
Abrasion 91mm³; DIN 53516
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 1.67 J/g-°C
Thermal Conductivity 0.280 W/m-KDIN 52612
Melting Point 220 °C
Maximum Service Temperature, Air 100 - 120 °Clong time operation
 120 - 140 °Cmedium time operation
 160 °Ca few hours operation
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 HB
 
Descriptive Properties
Time yield limitup to 5s1/1000; DIN.53444

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6)
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH
Zell-Metall Engineering Plastics Zellamid 1100 OIL
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH
Zell-Metall Engineering Plastics Zellamid 1100

PZELL18 / 72947

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.