MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Rogers Arlon 90B32R016AC Aluminum Clad Press Pad with "C-Finish"
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
  • Side 2: Alloy 1100 Aluminum Foil
  • Side 1: Cured Silicone Rubber

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccSilicone Property; Arlon SQA-TMS-024
 2.70 g/ccAlloy 1100 Property (Annealed)
Thickness 4.00 milLaminated Aluminum Foil; Arlon SQA-TMS-003
 12.0 milSide 1; Arlon SQA-TMS-003
 26.0 milOverall Thickness; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1481 psiSilicone Property; Arlon SQA-TMS-008
 12745 psiAlloy 1100 Property (Annealed); ASTM E345
Tensile Strength, Yield 4945 psiAlloy 1100 Property (Annealed); ASTM E345
Elongation at Break 263 %Silicone Property; Arlon SQA-TMS-008
Peel Strength 10.1 pliSilicone Compound Property - Adhesion Strength to Aluminum; Arlon SQA-TMS-011
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 - 300 °C
@Pressure 0.000 - 10.0 MPa
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 21.1 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al >= 99 %Alloy 1100
 
Descriptive Properties
Rigidity (grams)3500Arlon Gurley Test; Alloy 1100 Property (Annealed)
Total Product Weight (oz/yd2)19.5Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
1370 Aluminum
AISI 1095 Steel, oil quenched from 800°C (1475°F), 595°C (1100°F) temper
Aluminum 5052-H32
Cotronics Duralco™ 125 450°F Stress Free, Silver Filled Epoxy, Thermally Conductive
Oxygen-free Electronic Copper (OFE), UNS C10100, H10 Temper, flat products

PARL9813 / 148966

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.