PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 02535 is available in black or brown color. Information supplied by Plenco. |