MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Udel® P-1700 LCD PSU, Low viscosity for MF and UF membranes and microporous RO and NF substrates
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or spiral wound forms are also used. The membranes are used in a variety of applications, such as potable water treatment, waste water treatment, blood processing, pharmaceutical purification, gas separation, dairy product processing and for processing a variety of food products.

This resin offers the membrane producer good solubility in commercially available dipolar aprotic solvents, such as dimethylacetamide (DMAC), dimethylformamide, (DMF) and N-methyl pyrrolidone (NMP), which are completely miscible in water, very good control of pore size and pore size distribution, high membrane strength and good film-forming properties.

Typical grades of polysulfone contain a cyclic dimer that can precipitate from solution, plugging the process filters and limiting the life of the dope solutions. Udel® P-1700 NT LCD is specially manufactured to have a lower amount of cyclic dimer. It also has a higher number average molecular weight (Mn) for a given weight average molecular weight (Mw) leading to higher fiber strength, which means fewer fiber breakages, fewer surface defects and fewer rejects.

The resultant membranes have excellent hydrolytic stability and are compatible with pHs ranging from 2 to 13. They tolerate a variety of cleaning methods, including hydrochloric acid or sodium hydroxide. The resin has a Tg of 185°C indicating high thermal resistance.

- Transparent: Udel P-1700 NT LCD

Markets/Uses: Membranes / Membranes / Biomedical; Membranes / Membranes / Bioprocessing; Membranes / Membranes / Food and Beverage Processing; Membranes / Membranes / Gas Separation; Membranes / Membranes / Hemodialysis; Membranes / Membranes / Industrial Process Separations; Membranes / Membranes / RO/NF Composite Membrane Support Layer; Membranes / Membranes / UF/MF Low Pressure Water Filtration; Membranes / Membranes / Waste Treatment; Membranes / Membranes / Water Purification

Applications: Membranes

Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Chemical Resistant; Good Toughness; High Heat Resistance; Hydrocarbon Resistant; Hydrolytically Stable

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cmASTM D955
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 343 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 70.3 MPaASTM D638
Elongation at Break 50 - 100 %ASTM D638
Tensile Modulus 2480 MPaASTM D638
Flexural Strength 106 MPaASTM D790
Flexural Modulus 2690 MPaASTM D790
Izod Impact, Notched 69.0 J/mASTM D256
Tensile Impact Strength 420 kJ/m²ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+16 ohm-cmASTM D257
Dielectric Constant 3.02
@Frequency 1e+6 Hz
ASTM D150
 3.03
@Frequency 60 Hz
ASTM D150
 3.04
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.0011
@Frequency 60 Hz
ASTM D150
 0.0013
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 174 °CUnannealed; ASTM D648
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorTransparent - Slight Yellow
FormsPellets
ProcessingCoating; Extrusion; Injection Molding; Solution Processing
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4579 / 280379

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.