MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Crosspolimeri FRAGOM PR/04 AFKK N HFFR
Categories: Polymer; Thermoset

Material Notes: FRAGOM: is our brand of HFFR thermoplastic compounds having a very low flame propagation under fire conditions. Our Fragom is PVC free and also heavy-metals free.

FRAGOM PR/04 AFKK N: is designed to extrude both cable insulation and sheathing at high speed without any migration risks as it is completely free of plasticizers. Fragom PR/04 AFKKN meets the Australian Standard AS/NZ3808.2000 Insulation Type HFI-75-TP, HFI-90-TP, HFI-110-TP Sheathing Type HFS-75-TP,HFS-90-TP,HFS-110-TP

Certify: CEI2011 M1, VDE0207HM4(K=0,7), BS7655 LTS 3-4

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Melt Flow 6.0 - 12 g/10 min
@Load 21.6 kg,
Temperature 160 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 53ASTM D2240
Tensile Strength >= 10.0 MPaIEC 60811
 >= 12.5 MPa
@Temperature 110 °C,
Time 605000 sec
Heat Ageing; IEC 60811
Elongation at Break >= 170 %IEC 60811
 >= 212.5 %
@Temperature 110 °C,
Time 605000 sec
Heat Ageing; IEC 60811
Tear Strength >= 10.0 kN/mBS 6469-99-1
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.1
@Frequency 50 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 90.0 °C
@Time 21600 sec
<40%, Penetration; IEC 60811
Oxygen Index 30 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 130 °C
Zone 2 145 °C
Zone 3 160 °C
Zone 4 180 °C
Die Temperature 190 °C
Head Temperature 185 °C
Dry Time 3.00 hour
@Temperature 80.0 °C
 4.00 hour
@Temperature 90.0 °C
 
Descriptive Properties
Corrosivity of gases evolved>4,5 pHIEC 60754-2
Halogen Content0IEC 60754-1
Temperature Index Value>300°C21% O2, NES 715

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS079 / 294163

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.