MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 2200F Polyetherimide (PEI) (Americas)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Density 1.42 g/ccISO 1183
Water Absorption 0.19 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
 0.550 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.0 %ISO 62-1
 1.1 %ASTM D570
Viscosity 7.0 cP
@Load 5.00 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.0 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 114ASTM D785
Tensile Strength at Break 131 MPa5 mm/min; ASTM D638
 131 MPa5 mm/min; ISO 527
Tensile Strength, Yield 131 MPa5 mm/min; ASTM D638
 131 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ASTM D638
 2.0 %5 mm/min; ISO 527
Elongation at Yield 2.0 %5 mm/min; ASTM D638
 2.0 %5 mm/min; ISO 527
Tensile Modulus 6890 MPa5 mm/min; ASTM D638
 6890 MPa1 mm/min; ISO 527
Flexural Strength 225 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 228 MPayield, 2 mm/min; ISO 178
Flexural Modulus 6500 MPa2 mm/min; ISO 178
 6850 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 64.0 JASTM D256
 70.0 J
@Temperature -30.0 °C
ASTM D256
 464 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Unnotched 480 J/mASTM D4812
Izod Impact, Notched (ISO) 64.0 kJ/m²80*10*4; ISO 180/1A
 70.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 65.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 8.00 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+16 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 26.3 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
Dissipation Factor 0.0015
@Frequency 1000 Hz
ASTM D150
 0.0049
@Frequency 2.45e+9 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=3.00 mm
UL 746A
 15 - 30 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 60.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 208 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 212 °CRate B/50; ISO 306
 218 °CRate B/120; ISO 306
 220 °CRate B/50; ASTM D1525
UL RTI, Electrical 170 °CUL 746B
UL RTI, Mechanical with Impact 170 °CUL 746B
UL RTI, Mechanical without Impact 170 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.410 mm
UL 94
 5VA
@Thickness >=1.90 mm
UL 94
Oxygen Index 50 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °CInjection Molding
Mold Temperature 135 - 165 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82600 / 290547

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.