MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm Plexiglas® hw55 Clear Molding Compound
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Description: PLEXIGLAS® hw55 clear is a copolymer based on methyl methacrylate (MMA) with comonomer constituents. Besides showing the familiar properties of standard PLEXIGLAS® molding compound, such as
  • high light transmission
  • good flowability
  • high mechanical strength, surface hardness and abrasion resistance
  • excellent weatherability

PLEXIGLAS® hw55 clear offers the additional benefits of

  • increased heat deflection temperature under load
  • improved resistance to stress cracking
  • optimized inherent color

PLEXIGLAS® hw55 clear is particularly suitable for injection molding of technical items. Uses of PLEXIGLAS® hw55 clear: lighted keys, luminaire covers, fiber optics.

Information provided by degussa.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Moisture Absorption at Equilibrium 0.60 %Humidity Absorption (23°C, 50%); ISO 62
Water Absorption at Saturation 2.2 %Water Absorption in Water; ISO 62
Melt Flow 1.428 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPa5 mm/min; ISO 527
Elongation at Break 3.5 %5 mm/min; ISO 527
Tensile Modulus 3.60 GPa1 mm/min; ISO 527
Charpy Impact Unnotched 2.00 J/cm²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 109 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 106 °CISO 75
Vicat Softening Point 119 °CB50; ISO 306
Glass Transition Temp, Tg 122 °CIEC 10006
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 707
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.51ISO 489
Transmission, Visible 90 %Transmission Factor; DIN 5036
 
Processing PropertiesOriginal ValueComments
Processing Temperature 220 - 250 °CCylinder Temperature
Melt Temperature 220 - 250 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature <= 109 °CPredrying
Dry Time 2 - 3 hourDesiccant-type drier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® T65 XF Polycarbonate + ABS
Röhm ACRYLITE® hw55 Acrylic Polymer
Covestro Bayblend® T65 Polycarbonate + ABS
Trinseo Plexiglas® V052 Acrylic
Trinseo Plexiglas® V825 Acrylic

PHUK033 / 47167

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.