Geon HC 2155 is a 55 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2155 can be used for extrusion and injection molding healthcare applications. NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application. This product is not recommended for long-term storage of blood or blood components. Geon Performance Solutions was created from PolyOne in 2019. |