MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Polyamide PA66, reinforced with 30% of glass spheres, heat stabilized, for injection molding.

Available in: Europe

Product Applications: TECHNYL® A 218 S30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is recommended for mechanical components which require a very good surface finish with low warpage, and good compression strength. ( bearing housings ). This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183/A
Water Absorption 0.75 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527 Type 1A
Tensile Strength, Yield 80.0 MPaISO 527 type 1 A
Elongation at Break 9.0 %ISO 527 Type 1A
Elongation at Yield 4.0 %ISO 527 type 1 A
Tensile Modulus 4500 MPaISO 527 Type 1A
Flexural Modulus 3850 MPaISO 178
Izod Impact, Notched (ISO) 2.50 kJ/m²ISO 180/1A
Charpy Impact Unnotched 20.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 3.50 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+14 ohm-cmIEC 60093
Surface Resistance 5.00e+14 ohmIEC 60093
Dielectric Strength 30.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 450 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Oxygen Index 25 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 280 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY

PRHOD620 / 137851

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.