MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlbond™ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.

Application: Pearlbond™ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 2781
Viscosity 380000 cP
@Temperature 130 °C
Melt; ISO 1133
Melt Flow 60 - 100 g/10 min
@Load 2.16 kg,
Temperature 170 °C
ISO 1133
 
Chemical PropertiesOriginal ValueComments
Total Base Number <= 5.0mg KOH/g; MQSA 47 A
 
Thermal PropertiesOriginal ValueComments
Melting Point 60.0 - 64.0 °CMQSA 70 A
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.15 %MQSA 44
 
Descriptive Properties
Crystallization rate (minutes)9 - 11MQSA 12 B
ThermoplasticityVery highMQSA 68 A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Pearlbond® 1160 Thermoplastic Polyurethane
Lubrizol Advanced Materials Pearlbond® 580 Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 522 Linear Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 521 Linear Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 520 Linear Thermoplastic Polyurethane

PMES24 / 52922

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.