MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
NYCOA 534 H High Viscosity, Heat Stabilized Nylon 6 Resin
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: NYCOA 534 H is a high viscosity; heat stabilized, nucleated Nylon 6 resin. The high viscosity and fast set-up time make an excellent material for extrusion of tubing, rods, sheet and film. Because of its fast set-up time, fast extrusion line speeds have been achieved.

NYCOA 534 H is suitable for applications that require continuous exposure to temperatures in excess of 110° C.

Information provided by Nycoa, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Water Absorption 1.8 %24 hours; ASTM D570
Viscosity Measurement 4.0 - 4.4Relative, Sulfuric Acid; NYCOA test
 145 - 200Relative, Formic Acid; NYCOA test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D785
Tensile Strength, Yield 83.0 MPaASTM D638
Elongation at Break 130 %ASTM D638
Flexural Strength 114 MPaASTM D790
Flexural Modulus 2.689 GPaASTM D790
Izod Impact, Notched 59.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 221 °CASTM D789
Maximum Service Temperature, Air 110 °C
Deflection Temperature at 0.46 MPa (66 psi) 191 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °CASTM D648
 
Descriptive Properties
Water Extractables, %0.8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NYCOA 534H PA 6
NYCOA 589 PA 6
NYCOA 578 PA 6
NYCOA 567 PA 6
NYCOA 5100 HS Heat Stabilized, Impact Modified Nylon 66 Resin

PNYCO09 / 55544

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.