Moplen EF300N is a medium flow flake form copolymer for compounding applications. It offers a good stiffness/impact balance and has a fine and very regular particle size distribution. Moplen EF300N is designed for production of compounds and master batches. Typical applications are color and additives master batches, mineral filled compounds and woodstock.Information provided by LyondellBasell. |